Differential Scanning Calorimetry (DSC) is a thermal analysis technique that looks at how a material’s heat capacity is changed by temperature. During heating or cooling a sample, the changes in its heat capacity are registered as changes in the heat flow. DSC is one of the most important tool for thermal analysis, which allows to measure:
- heat and temperature of phase transitions like melting and crystallization
- degree of crystallinity
- glass transition temperature
- kinetics of phase transitions
- heat capacity
- thermal conductivity
Our DSC is equipped with intracooler (temperature range -65oC to 550oC).